Apr 24, 20090183325. Immerse the part into the bath and allow to soak for 1 hour bigger thickness of steel will of course need longer. 6. Allow 3 hours for the carburization process. This usually gives about 1 mm to 2 mm of case hardening. 7. 4140 cannot be carburized using this method. You need to use steel made for the purpose EN36A, etc. 8.